  "jsonld": {
    "@context": "https://schema.org",
    "@type": "Dataset",
    "about": {
      "@type": "ChemicalSubstance",
      "chemicalComposition": "LiNbO3",
      "name": "lithium niobate"
    },
    "citation": [],
    "creator": {
      "@type": "Person",
      "name": "Wentao Jiang"
    },
    "description": "Residual absorption, as-grown crystals of lithium niobate (LiNbO3): 1 provenance-tagged value(s) from 1 source(s) for variant(s) cln. Each value carries conditions, uncertainty, the source locator and a status code (P primary, P-comp compilation, P-db database, S secondary, V vendor, C computed).",
    "distribution": [
      {
        "@type": "DataDownload",
        "contentUrl": "https://lithium-niobate.com/api/v1/properties/residual-absorption.json",
        "encodingFormat": "application/json"
      },
      {
        "@type": "DataDownload",
        "contentUrl": "https://lithium-niobate.com/api/v1/properties.csv",
        "encodingFormat": "text/csv"
      }
    ],
    "identifier": "https://lithium-niobate.com/api/v1/properties/residual-absorption.json",
    "isAccessibleForFree": true,
    "keywords": [
      "lithium niobate",
      "LiNbO3",
      "Residual absorption, as-grown crystals"
    ],
    "license": "https://creativecommons.org/licenses/by/4.0/",
    "name": "LiNbO3 Residual absorption, as-grown crystals",
    "url": "https://lithium-niobate.com/api/v1/properties/residual-absorption.json",
    "variableMeasured": [
      {
        "@type": "PropertyValue",
        "measurementTechnique": "see source",
        "name": "Residual absorption, as-grown crystals (cln)",
        "unitText": "/cm",
        "value": "up to 0.04 cm^-1 (transition-metal impurities, 400-2000 nm); about 0.001 cm^-1 H-related bands at 2300-2800 nm; annealing lowers absorption by up to 10x"
      }
    ],
    "version": "0.1.0"
  },
  "meta": {
    "api_version": "v1",
    "attribution": "lithium-niobate.com data compiled by Wentao Jiang; cite the original sources listed per value.",
    "count": 1,
    "data_version": "0.1.0",
    "documentation": "https://lithium-niobate.com/api/openapi.json",
    "license": {
      "id": "CC-BY-4.0",
      "name": "Creative Commons Attribution 4.0 International",
      "url": "https://creativecommons.org/licenses/by/4.0/"
    },
    "property": "residual-absorption"
  },
  "records": [
    {
      "category": "optical",
      "default": true,
      "id": "residual-absorption/cln/schwesyg2011",
      "kind": "scalar",
      "name": "Residual absorption, as-grown crystals",
      "property": "residual-absorption",
      "provenance": {
        "locator": "abstract; Sec. 3.1, 3.3",
        "source_id": "schwesyg2011",
        "status": "P",
        "transcribed": "2026-10-25"
      },
      "public": true,
      "unit": {
        "display": "cm^-1",
        "ucum": "/cm"
      },
      "value_text": "up to 0.04 cm^-1 (transition-metal impurities, 400-2000 nm); about 0.001 cm^-1 H-related bands at 2300-2800 nm; annealing lowers absorption by up to 10x",
      "variant": "cln",
      "variant_note": "CLN and MgO5 crystals"
    }
  ]
}